Wednesday, April 16, 2008

Stellite coating on PM tools and impeller

Idea....immerse tool in a thick hydroxide slurry .... hydroxide metals
same ratio as stellite composition. May need to work on ways to get
slurry to stick to iron, but don't need a thick coating. Remove tool,
let it dry, and bake coating on in oven. Could even dip it in syrup and
then bake it to get hard coating. Then add 625M PM or similar. During
hipping oxide reduced to metal by iron and syrup.
Kind regards,

Robert

Robert R. Odle, Ph.D.
Consultant
443-616-4339
www.metallurgicalviability.com

Experienced in (1) PROCESS ENGINERRING & ECONOMICS, (2) CORROSION AND
(3) FAILURE ANALYSIS. Seeking consulting and/or profit and loss
responsibility.

No comments: